美国对于列车防火安全要求类同于欧洲主要国家列车防火安全要求,即限定材料的阻燃性能,对于不同材料又有不同测试方法。以此来防止火灾的发生或者延迟火灾的发展及蔓延。
联邦铁路管理规定(FRA)
索引 |
部件分类 |
材料分类 |
测试方法 |
性能标准 |
|
衬垫 |
|
ASTM D-3675 |
Is<= 25 |
ASTM E-662 |
Ds (1.5) < 100 | |||
|
织物 |
|
14CFR, 附件 F, |
燃烧时间< 10 s |
ASTM E-662 |
Ds(4) < 200 | |||
ASTM E-162 |
Is <= 35 | |||
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 200 | |||
ASTM D-3675 |
Is <= 25 | |||
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 175 | |||
ASTM E648 |
CRF> 5 kW/m2 | |||
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 200 | |||
ASTM E-162 |
Is <= 100 | |||
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 200 | |||
平均燃烧传播(垂直测试) |
略 | |||
NEMA WC3/ICEA S-19-1981, 章节 |
略 | |||
ASTM E-662 |
Ds(4) < 200 (燃烧) | |||
ANSI/IEEE Std 383 |
Pass | |||
ASTM E-662 |
Ds(4) < 200 (燃烧) | |||
ASTM E119 |
略 | |||
|
|
|
|
|
|
车辆组件 |
除了泡沫塑料、地板垫、透光塑料以及分类1和2中列举的项目之外的所有材料 |
ASTM E-162 |
Is <= 35 |
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 200 | |||
柔软的泡沫塑料 |
ASTM D-3675 |
Is <= 25 | ||
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 175 | |||
地板垫 |
ASTM E648 |
CRF> 5 kW/m2 | ||
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 200 | |||
透光塑料 |
ASTM E-162 |
Is <= 100 | ||
ASTM E-662 |
Ds(1.5) < 100, Ds(4) < 200 | |||
弹性体 |
平均燃烧传播(垂直测试) |
略 | ||
|
电线及电缆 |
低电压电线电缆: 控制电路中的绝缘线及其它低于100 V AC和150 V DC的低压电缆 |
NEMA WC3/ICEA S-19-1981, 章节 |
略 |
ASTM E-662 |
Ds(4) < 200 (燃烧) | |||
电源线: 控制电路中的绝缘线及其它高于100 V AC and150 V DC的电缆 |
ANSI/IEEE Std 383 |
Pass | ||
ASTM E-662 |
Ds(4) < 200 (燃烧) | |||
|
结构组件 |
地板, 其它 |
ASTM E119 |
略 |
地板材料辐射板测试或者“使用辐射热源测试地面材料临界热通量的标准测试方法ASTM E 648是将一块样品水平暴露在一个辐射热源下面,这个辐射热源长度为 |